This is layer 2 or 3. It will be covered by the next few layers but I feel like it shouldn’t be this fugly. I’m using Cura’s Standard Quality except for temp which is set to 205. The filament is Inland PLA.
This is layer 2 or 3. It will be covered by the next few layers but I feel like it shouldn’t be this fugly. I’m using Cura’s Standard Quality except for temp which is set to 205. The filament is Inland PLA.
z offset / nozzle height seems to be the thing. I’ve raised it up and it looks better. After that I played with the temp a bit and it seems to be happier around 210-215 though there is more stringing.
So far, all attempts at ironing have been a disaster, both zig zag and concentric. I’m going to continue dialing in the z offset and temp before ironing.