This was an ornament I printed roughly 6 years ago. Being a Christmas ornament it spent most of those 6 years stored in my roof space.

Being in Australia this would have been subject to average temperatures of 30 to 35 degrees c but also peaks across summer approaching 70 degrees c. Also in high humidity.

The PLA crumbles into tiny pieces at the softest touch.

I thought it was interesting that PLA would start to break down in these conditions.

  • eramseth@lemmy.world
    link
    fedilink
    English
    arrow-up
    3
    ·
    11 days ago

    Heat and humidity. Humidity more than the heat in my experience. Spools of pla get brittle if left in a humid environment.