Which is to say, not very far on this at all but I think I have a good idea on how have my cake and eat it too for desiccant for my spools.

I am finding I can’t get the humidity below about 50% in my AMS and the silica I am using needs constant refreshing.

Well it seems there is stuff called activated alumina that is pretty good and honestly about the same costs as silica beads, but I need to be able to put it in the oven to refresh it. Which doesn’t work well with my 3d printed desiccant holders.

Insert, cheap tea strainers.
It seems I can get ones that are 4cm in width by 6cm in height that are made out of stainless steel that I can actually put straight in the oven.

So, I am working on getting the parts and items but was wondering if anyone else has done this or have any suggestions before I start grabbing stuff?

  • Grippler@feddit.dk
    link
    fedilink
    English
    arrow-up
    5
    ·
    7 days ago

    but I don’t think my oven maintains low temperatures well enough to not melt the beads.

    You must have a pretty insane oven there, because silica dioxide (which is what they’re made of) melts at 1700°C (3100°F)